Compared with the cored wire, the solid core wire has higher strength, better compactness and high calcium content. It can feed calcium to the deeper part of molten steel and stay below the critical depth for a longer time, s
1) The calcium recovery rate is improved. After feeding the solid pure calcium cored wire developed by our factory, the average calcium recovery rate of low-carbon
Calcium is the strongest deoxidizer used in steelmaking so far. In molten steel, calcium has a unique chemical connection with dissolved oxygen and total oxygen in non-metallic inclusions.
Phone
+86-0538-8109178
Sales:Maodong Ji Mobile:+86 133 8538 3909 Wechat/Whatsapp:+86 133 8538 3909 Email:sales03@sdgyxcl.com Address:No. 5 Angang Street, Manzhuang Steel Market, Daiyue District, Tai’an City, Shandong Province