The process and parameters of composite pure calcium wire are summarized
Hits:     Date:2017-8-7 11:02:39

The process and parameters of composite pure calcium wire are summarized

Guoyi new material determines the amount of wire feeding according to the end-point smelting of molten steel and aluminum deoxidation, and has reached the appropriate aluminum calcium ratio. Timely adjust the pressure of the wire feeding wheel of the wire feeder to ensure that the wire feeder does not slip during the wire feeding process. Make the automatic counting of the wire feeder accurate and reliable, so as to master the reliable wire feeding quantity. Adjust the wire feeding speed according to the size of the ladle to reduce the churning and oxidation of molten steel, so as to feed the wire smoothly.

Composite pure calcium line parameters:

Main composition: Ca ≥ 52g / M

Diameter: 9 ± 0.25mm

Dosage: 0.35-0.4kg/ton steel

Speed: 1.5-2m \ s 9mm

The model of seamless calcium wire is 9, 10 and 12 seamless composite calcium wires

Ad powder is 10, 15, 20, 25... 60al

Aluminum ash is 10, 15, 20, 25... 60al

The aluminum particle is 95-99.5al

The aluminum chip is 90-97al

The deoxidation ball is 10-40al

Ad ball is 10-40al

The above content introduces the process and parameters of composite pure calcium wire. More wonderful knowledge of composite pure calcium wire is in Guoyi new material company.

Previous:The principle and ...          Next:The technology of ...
Other Product
News Center
Phone
+86-0538-8109178

Sales:Maodong Ji
Mobile:+86 133 8538 3909
Wechat/Whatsapp:+86 133 8538 3909
Email:sales03@sdgyxcl.com
Address:No. 5 Angang Street, Manzhuang Steel Market, Daiyue District,
Tai’an City, Shandong Province


SCAN ADD WECHAT